Corrosion Treatment
Stopping Deterioration at the Steel
Reinforcement corrosion is the most common cause of concrete deterioration in the UAE, driven by chlorides and carbonation. HAVEN FORCE treats the steel itself and then protects the element so the process does not simply restart.
Steel
Cleaned
Passivating
Primer
Chloride
Assessment
Long-Term
Protection
What We Typically Find
The conditions most often reported before a corrosion treatment scope is developed.
Rust staining bleeding through concrete
Corrosion products expanding and forcing their way out.
Cracking along reinforcement lines
Expansion of corroding steel splitting the cover concrete.
Exposed, section-losing rebar
Steel that has lost cross-sectional area and strength.
Corrosion restarting after repair
Chlorides left in the surrounding concrete continuing the process.
What This Service Covers
Service Scope
- Condition survey and cover meter scan
- Half-cell potential and chloride testing where specified
- Breaking out around affected reinforcement
- Abrasive cleaning of steel to bright metal
- Supplementary reinforcement where section is lost
- Passivating or zinc-rich primer application
- Repair mortar reinstatement
- Anti-carbonation protective coating
Suitable For
- Commercial Buildings
- Car Parks & Podiums
- Industrial Facilities
- Retaining Walls
- Water Retaining Structures
- Residential Developments
- Balconies & Facades
- Infrastructure Elements
Key Benefits
- Treats the cause, not the symptom
- Passivates the reinforcement
- Informed by testing
- Slows future deterioration
- Restores lost section where needed
- Reduces repeat repair cycles
- Improves structural safety
- Extends asset life
Work Methodology
Five controlled stages from first inspection to final quality check.
1
Survey & Test
Scan cover, map defects and test for chlorides and carbonation depth.
2
Break Out
Remove concrete around the affected steel, fully exposing its circumference.
3
Steel Cleaning
Abrasive-clean to bright metal and add supplementary bars if section is lost.
4
Priming
Apply zinc-rich or cementitious passivating primer to the cleaned steel.
5
Reinstate & Protect
Reinstate with repair mortar and apply an anti-carbonation coating.
Specified To The Condition
Systems are selected according to substrate, exposure and project specification. The final specification is confirmed after a site assessment.
Zinc-Rich Primer
Sacrificial coating that protects the steel electrochemically.
Cementitious Passivator
Restores a high-alkalinity environment around the reinforcement.
Migrating Corrosion Inhibitor
Penetrates the concrete to reach steel beyond the repair area.
Questions About Corrosion Treatment
Related Concrete Repair Services
Concrete Repair
Restoring Damaged Concrete
ViewCrack Repair
Closing the Path Through Concrete
ViewMicro Concrete Repair
Flowable Repair for Larger Sections
ViewStructural Strengthening
Adding Capacity to Existing Structures
ViewHoneycomb Repair
Filling Voids Left by the Pour
ViewProtective Coating
Slowing the Next Cycle of Decay
View