Dry Crack Injection by HAVEN FORCE Technical Services in Dubai
Leakage & Injection

Dry Crack Injection

Restoring Dormant Cracks

A dry, non-moving crack can be bonded back together with epoxy so the element regains its structural continuity. HAVEN FORCE injects dormant cracks in slabs, beams, columns and walls to restore strength and close the moisture path.

Dormant
Cracks

Structural
Bond

Full-Depth
Penetration

Permanent
Repair

Common Problems

What We Typically Find

The conditions most often reported before a dry crack injection scope is developed.

01

Cracking through a structural member

Loss of continuity affecting how load is carried.

02

Shrinkage cracks in a new slab

Early-age cracking that needs sealing before services are installed.

03

Cracks admitting moisture to rebar

Open paths that will eventually start corrosion.

04

Cracking after settlement

Movement that has since stabilised but left the element cracked.

Scope & Application

What This Service Covers

Service Scope

  • Crack survey and movement monitoring
  • Confirmation that the crack is dry and dormant
  • Surface cleaning and crack mapping
  • Port installation and surface sealing
  • Low-viscosity epoxy injection
  • Port removal and grinding flush
  • Core verification where specified
  • Documentation and handover

Suitable For

  • Basements
  • Retaining Walls
  • Construction Joints
  • Lift Pits
  • Water Tanks & Reservoirs
  • Swimming Pools
  • Podiums & Underground
  • Tunnels & Utility Ducts

Key Benefits

  • Restores structural continuity
  • Bond stronger than the concrete
  • Closes the moisture pathway
  • Protects reinforcement
  • Permanent and non-shrinking
  • Penetrates very fine cracks
  • Verifiable by core sampling
  • Avoids member replacement
Our Process

Work Methodology

Five controlled stages from first inspection to final quality check.

Inspection — Dry Crack Injection
1

Inspection

Confirm the crack is dry and has stopped moving, and map its extent.

Port Installation — Dry Crack Injection
2

Port Installation

Fix ports along the crack and seal the surface between them.

Injection — Dry Crack Injection
3

Injection

Inject low-viscosity epoxy from the lowest port until refusal.

Finishing — Dry Crack Injection
4

Finishing

Cure fully, remove ports and grind the surface flush.

Verification — Dry Crack Injection
5

Verification

Core sample or ultrasonic check where specified.

Materials & Systems

Specified To The Condition

Systems are selected according to substrate, exposure and project specification. The final specification is confirmed after a site assessment.

Low-Viscosity Epoxy

Capillary action carries it into cracks well below a millimetre wide.

Surface Seal Paste

Contains injection pressure so resin travels along the crack, not out of it.

Injection Ports

Spaced to the element thickness so resin reaches full depth.

Gallery

Work In Progress

Dry Crack Injection — site photograph
View
Dry Crack Injection — site photograph
View
Dry Crack Injection — site photograph
View
Dry Crack Injection — site photograph
View
Full Gallery
FAQs

Questions About Dry Crack Injection

By monitoring it, often with tell-tales, over a period. Injecting a live crack with rigid epoxy will simply crack again alongside.
Epoxy will not bond to a wet substrate. The crack is dried, or a PU or acrylic system is used instead.
Ports are removed and the surface ground flush. A fine line may remain visible unless the surface is coated.
WhatsApp Call Us