Structural Bonding for Dry Cracks

Epoxy injection restores the structural continuity of concrete by bonding a dry, dormant crack back together. The cured resin is stronger than the surrounding concrete, so the element behaves as a monolith again.

Structural
Bonding

High
Strength

Dormant
Cracks

Permanent
Repair

Common Problems

What We Typically Find

The conditions most often reported before a epoxy injection scope is developed.

01

Structural cracks through a member

Loss of continuity affecting how the element carries load.

02

Cracking after overload or impact

Damage that needs strength restored, not just sealing.

03

Shrinkage cracks in slabs and walls

Dormant cracks that reduce durability and admit moisture.

04

Delamination between concrete layers

Separation that needs re-bonding to act together.

Scope & Application

What This Service Covers

Service Scope

  • Crack survey and movement check
  • Surface cleaning and crack mapping
  • Port installation at calculated spacing
  • Surface sealing between ports
  • Low-viscosity epoxy injection
  • Port removal and surface grinding
  • Verification by core or ultrasonic check where specified
  • Documentation and handover

Suitable For

  • Basements
  • Retaining Walls
  • Construction Joints
  • Lift Pits
  • Water Tanks & Reservoirs
  • Swimming Pools
  • Podiums & Underground
  • Tunnels & Utility Ducts

Key Benefits

  • Restores structural continuity
  • Cured resin exceeds concrete strength
  • Improves load transfer
  • Permanent, non-shrinking repair
  • Penetrates very fine cracks
  • Avoids member replacement
  • Verifiable by core sampling
  • Suitable for critical elements
Our Process

Work Methodology

Five controlled stages from first inspection to final quality check.

Inspection — Epoxy Injection
1

Inspection

Confirm the crack is dry and dormant, and map its full extent.

Port Installation — Epoxy Injection
2

Port Installation

Fix injection ports along the crack at calculated spacing.

Injection Application — Epoxy Injection
3

Injection Application

Inject low-viscosity epoxy from the lowest port upward until refusal.

Curing & Finishing — Epoxy Injection
4

Curing & Finishing

Allow full cure, remove ports and grind the surface flush.

Final Inspection — Epoxy Injection
5

Final Inspection

Verify penetration and quality, by core sample where specified.

Materials & Systems

Specified To The Condition

Systems are selected according to substrate, exposure and project specification. The final specification is confirmed after a site assessment.

Low-Viscosity Epoxy

Flows into hairline cracks by capillary action and cures rigid.

Injection Ports

Surface-mounted or drilled ports depending on crack width and access.

Surface Seal Paste

Temporary epoxy paste that contains the injection pressure along the crack.

Gallery

Work In Progress

Epoxy Injection — site photograph
View
Epoxy Injection — site photograph
View
Epoxy Injection — site photograph
View
Epoxy Injection — site photograph
View
Full Gallery
FAQs

Questions About Epoxy Injection

No. Epoxy needs a dry substrate to bond. If the crack is wet or moving, PU or acrylic is the correct choice.
The cured epoxy is. A correctly injected crack will typically fail elsewhere in the concrete rather than at the repair.
Injection proceeds port to port until resin appears at the next one, and cores can confirm penetration where specified.